T/C
1. Composition: T/C 65/35
2. Yarn count: 21x16
3. Density: 120x60
4. Width: 58/60"
Full process
1. Level of color fastness to
1.1 water 4-5
1.2 light 4+
1.3 soaping 4+
1.4 dry rubbing 4+
1.5 wet rubbing 3-4
2. Color difference level 4+
3. Singeing level 4+
4. Finishing (MOQ 3000m/color)
4.1 softening
4.2 water proof
4.3 anti-static
4.4 fire resistant finish
4.5 teflon (waterproof, oil proof, anti-fouling)
4.6 wicking finish
4.7 anti-UV
4.8 noniron finish
4.9 starch finish
4.10 anti-bacterial
4.11 mothproof finish
4.12 increasing weight finish
1. Composition: T/C 65/35
2. Yarn count: 21x16
3. Density: 120x60
4. Width: 58/60"
Full process
1. Level of color fastness to
1.1 water 4-5
1.2 light 4+
1.3 soaping 4+
1.4 dry rubbing 4+
1.5 wet rubbing 3-4
2. Color difference level 4+
3. Singeing level 4+
4. Finishing (MOQ 3000m/color)
4.1 softening
4.2 water proof
4.3 anti-static
4.4 fire resistant finish
4.5 teflon (waterproof, oil proof, anti-fouling)
4.6 wicking finish
4.7 anti-UV
4.8 noniron finish
4.9 starch finish
4.10 anti-bacterial
4.11 mothproof finish
4.12 increasing weight finish
Polyester Cotton Twill Fabric | |||
T/C 80/20 | 21sX16s | 128X60 | 57/58/59/60' ' |
21sX21s | 108X58 | ||
T/C 65/35 | 14sX14s | 80X52 | 57/58/59/60' ' |
16sX12s | 108X56 | ||
21sX16s | 128X60 | ||
21sX21s | 108X58 | ||
32sX32s | 130X70 | ||
CVC 55/45 60/40 | 21sX16s | 128X60 | 57/58/59/60' ' |
32sX32s | 130X70 |